o Ti o dara ju Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Pipe Pipe, Sheet, Waya olupese ati Olupese |Guojin

Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Paipu Alailẹgbẹ, Sheet, Waya

Apejuwe kukuru:

Iwọn deede:
UNS N07750
DIN W. Nr.2.4669


Alaye ọja

ọja Tags

Awọn ọja to wa

tube Ailokun, Awo, Rod, Forgings, fasteners, Pipe Fittings

Awọn ajohunše iṣelọpọ

Ọja

ASTM

Ifi ati Forgings

B637

Kemikali Tiwqn

%

Ni

Cr

Fe

C

Mn

Si

S

Ti

Nb+Ta

Al

Co

Cu

Min

70.0

14.0

5.0

2.25

0.70

0.40

O pọju

17.0

9.0

0.08

1.00

0.50

0.010

2.75

1.20

1.00

1.00

0.50

Ti ara Properties

iwuwo

8,28 g / cm3

Yiyọ

1393-1427 ℃

Inconel X-750 Awọn ẹya ara ẹrọ

Inconel X-750 alloy jẹ nipataki superalloy ti o da lori nickel eyiti o jẹ alagbara ọjọ-ori pẹlu ipele γ[Ni3(Al, Ti, Nb)].O ni o ni ti o dara ipata resistance ati ifoyina resistance ni isalẹ 980 ℃, ati ni isalẹ 800 ℃ O ni o ni ga ipata resistance.O ni o ni ti o dara isinmi resistance ni isalẹ 540 ° C, bi daradara bi ti o dara formability ati weldability.A lo alloy yii ni pataki fun iṣelọpọ awọn ẹrọ ọkọ ofurufu ti o ṣiṣẹ ni isalẹ 800 ° C ati nilo agbara giga..Awọn orisun omi tun le ṣee ṣe lati ṣe iṣelọpọ awọn abẹfẹlẹ turbine nya si ati awọn ẹya miiran, gẹgẹbi awọn awo, awọn ila, awọn ifi, awọn ayederu, awọn oruka, awọn onirin, awọn paipu, ati bẹbẹ lọ.

Inconel X-750 Ooru Itọju Ilana

Eto itọju ooru ojutu fun awọn awopọ, awọn ila ati awọn paipu ni ipo ipese jẹ 980 ℃ ± 15 ℃, itutu agbaiye afẹfẹ.Fun eto itọju ooru agbedemeji ti awọn ohun elo ati awọn ẹya, awọn ilana atẹle le ṣee yan fun itọju ooru.
Annealing: 955 ~ 1010 ℃, omi itutu agbaiye.
Annealing ti welded awọn ẹya ara ṣaaju ki o to alurinmorin: 980 ℃, 1h.
Iderun iderun annealing ti welded awọn ẹya ara: 900 ℃, moisturizing fun 2h.
Annealing iderun wahala: 885 ± 15 ℃, 24h, air itutu.

Inconel X-750 Wa Awọn oriṣiriṣi ati Awọn pato

Awọn ifi, awọn ayederu, awọn oruka, awọn iwe ti a ti yiyi ti o gbona, awọn aṣọ ti o tutu, awọn ila, awọn tubes ati awọn okun waya le wa ni awọn titobi pupọ.
Awọn awo ati awọn ila ni gbogbo igba ti pese lẹhin ti o gbona tabi tutu yiyi, annealing tabi ojutu, gbigbe ati didan.
Awọn ifi, awọn ayederu ati awọn oruka le wa ni ipese ni ayederu tabi ipo yiyi gbona;wọn tun le pese ni itọju ojutu lẹhin sisọ;Awọn ifi le wa ni ipese lẹhin ojutu ati didan tabi titan, ati pe o le pese ni otutu nigbati aṣẹ ba nilo Fa ipo si aaye.
Awọn waya le wa ni pese ni ri to ojutu ipinle;fun okun waya pẹlu iwọn ila opin tabi sisanra ni isalẹ 6.35mm, o le jẹ ojutu to lagbara ati pese pẹlu abuku iyaworan tutu ti 50% si 65%;awọn ipin opin tabi ẹgbẹ ipari jẹ tobi ju 6.35mm.Waya, lẹhin itọju ojutu, ti pese pẹlu abuku iyaworan tutu ti ko kere ju 30%.Fun awọn okun onirin pẹlu iwọn ila opin tabi ipari ẹgbẹ ko tobi ju 0.65mm, wọn le pese pẹlu abuku iyaworan tutu ti ko din ju 15% lẹhin itọju ojutu bi o ṣe nilo.

Inconel X-750 Awọn agbegbe Ohun elo

A lo alloy ni akọkọ fun iṣelọpọ awọn orisun ewe ati awọn orisun okun pẹlu awọn ibeere agbara giga ati resistance isinmi fun awọn ẹrọ aero-ero ti n ṣiṣẹ ni isalẹ 800 ° C.O tun le ṣee lo lati ṣe awọn ẹya bii awọn abẹfẹlẹ tobaini.Awọn orisirisi ti o wa ni dì, rinhoho, igi, ayederu, oruka, waya ati tube.