Superalloy Inconel625/ UNS N06625/ Aloy625 Olupese
Awọn ọja to wa
tube Ailokun, Awo, Rod, Forgings, fasteners, Pipe Fittings
Awọn ajohunše iṣelọpọ
Ọja | ASTM |
Pẹpẹ | B446 |
Awo, Dì ati rinhoho | B 443, B 906 |
Paipu ailopin, tube | B 444, B 829 |
welded paipu | B 705, B 775 |
Awọn ohun elo welded | B 704, B 751 |
welded asopo | B 366 |
Eke billets ati ifi | B472 |
Ṣiṣẹda | B 564 |
Kemikali Tiwqn
% | Ni | Cr | Mo | Fe | C | Mn | Si | P | S | Co | Nb+Ta | Al | Ti |
Min | 58.0 | 20.0 | 8.0 |
|
|
|
|
|
|
| 3.15 |
|
|
O pọju |
| 23.0 | 10.0 | 5.0 | 0.10 | 0.50 | 0.50 | 0.015 | 0.015 | 1.00 | 4.15 | 0.40 | 0.40 |
Ti ara Properties
iwuwo | 8.36g/cm3 |
Yiyọ | 1330-1375 ℃ |
Inconel 625 Awọn ẹya ara ẹrọ
1. Iyatọ ipata ti o dara julọ si ọpọlọpọ awọn media ibajẹ ni oxidizing ati idinku awọn agbegbe
2. O tayọ resistance si pitting ipata ati crevice ipata, ati ki o yoo ko gbe awọn kiloraidi ion wahala ipata wo inu.
3. O tayọ ipata resistance si inorganic acids, gẹgẹ bi awọn nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid ati adalu acids ti sulfuric acid ati hydrochloric acid, ati be be lo.
4. O tayọ resistance si ipata ti awọn orisirisi inorganic acid adalu solusan
5. Nigbati awọn iwọn otutu Gigun 40 ℃, o le fi ti o dara ipata resistance ni orisirisi awọn ifọkansi ti hydrochloric acid ojutu
6. Ti o dara workability ati weldability, ko si post-weld wo inu ifamọ
7. Ijẹrisi iṣelọpọ ti awọn ohun elo titẹ pẹlu iwọn otutu odi ti -196~450℃
8. Ifọwọsi nipasẹ American Society of Corrosion Engineers NACE boṣewa (MR-01-75) lati pade ipele ti o ga julọ VII fun lilo ni awọn agbegbe gaasi ekan.
Inconel625 Awọn agbegbe Ohun elo
Awọn rirọ ati annealed kekere carbon alloy 625 ti wa ni o gbajumo ni lilo ninu awọn kemikali ilana ile ise, ati awọn oniwe-dara ipata resistance ati ki o ga agbara jeki o lati ṣee lo bi awọn tinrin igbekale paati.Alloy 625 le ṣee lo ni awọn ohun elo ti o farahan si omi okun ati koko-ọrọ si aapọn ẹrọ giga.Awọn agbegbe ohun elo ti o wọpọ:
1. Awọn paati ti awọn ilana kemikali Organic ti o ni awọn chlorides, paapaa nibiti a ti lo awọn ayase kiloraidi acid
2. Digesters ati awọn tanki bleaching fun awọn ti ko nira ati iwe ile ise
3. Ile-iṣọ gbigba, reheater, flue gas inlet baffle, fan (ọrinrin), agitator, deflector ati flue ni flue gas desulfurization system
4. Fun iṣelọpọ ẹrọ ati awọn paati fun lilo ninu awọn agbegbe gaasi ekan
5. Acetic acid ati acetic anhydride lenu monomono
6. Sulfuric acid condenser